Amanqaku aphambili enkqubo yokuvelisa ibhegi yefoyile ye-aluminium

1, Ukwenziwa kwe-Anilox Roller kwiMveliso ye-Aluminium Foil Bag,
Kwinkqubo yokulaminatha okomileyo, kufuneka iiseti ezintathu zeerola ze-anilox ukuze kuncamathiselwe iirola ze-anilox:
Imigca 70-80 isetyenziselwa ukuvelisa iipakethi zokuziphinda-phinda ezineglu eninzi.
Umgca we-100-120 usetyenziselwa ukupakisha iimveliso ezimelana nobushushu obuphakathi ezifana namanzi abilayo.
Imigca 140-200 isetyenziselwa ukuvelisa iimveliso zokupakisha ngokubanzi ezingenaglue ingako.

2, iiparameter eziphambili zeComposite ekuvelisweni kweengxowa zefoyile ye-aluminiyam
Ubushushu be-oven: 50-60℃;60-70℃;70-80℃。
Ubushushu bomqulu odibeneyo: 70-90℃.
Uxinzelelo oluhlanganisiweyo: Uxinzelelo lwerola edibeneyo kufuneka lonyuswe kangangoko kunokwenzeka ngaphandle kokutshabalalisa ifilimu yeplastiki.
Malunga neemeko ezithile ezithile:
(1) Xa ifilimu ecacileyo ilaminethiwe, ubushushu be-oven kunye ne-roller ye-laminating kunye nomoya ophuma kwi-oven (umthamo womoya, isantya somoya) zinempembelelo enkulu ekukhanyeni. Xa ifilimu eprintayo iyi-PET, kusetyenziswa ubushushu obuphantsi; xa ifilimu eprintayo iyi-BOPP.
(2) Xa kudityaniswa ifoyile ye-aluminiyam, ukuba ifilimu yokuprinta yi-PET, ubushushu berola edibanisayo kufuneka bube ngaphezulu kwama-80℃, buqhele ukulungiswa phakathi kwama-80-90℃. Xa ifilimu yokuprinta iyi-BOPP, ubushushu berola edibanisayo akufuneki budlule kuma-8

1

3, iingxowa zefoyile ziyanyangeka ngexesha lemveliso.
(1) ubushushu bokuphilisa: 45-55℃.
(2) ixesha lokunyanga: iiyure ezingama-24-72.
Faka imveliso kwigumbi lokuthambisa kwi-45-55°C, iiyure ezingama-24-72, ngokubanzi iintsuku ezimbini zeengxowa ezicacileyo, iintsuku ezimbini zeengxowa zefoyile ye-aluminium, kunye neeyure ezingama-72 zeengxowa zokupheka.

3

4. Ukusetyenziswa kweglu eseleyo ekuvelisweni kweengxowa zefoyile ye-aluminium
Emva kokuxuba isisombululo serabha esisele kabini, sivale, kwaye ngosuku olulandelayo, faka isisombululo serabha esitsha njengesinyibilikisi, xa kufuneka imveliso ephezulu, kungabi ngaphezu kwe-20% yetotali iyonke, ukuba iimeko zingcono ukugcina efrijini. Ukuba umswakama we-solvent uyafaneleka, i-glue elungisiweyo iya kugcinwa iintsuku ezi-1-2 ngaphandle kotshintsho olukhulu, kodwa ekubeni ifilimu edibeneyo ingenakugwetywa ngoko nangoko ukuba iyafaneleka okanye ayifanelekanga, ukusetyenziswa ngokuthe ngqo kweglue eseleyo kunokubangela ilahleko enkulu.

2

5. Iingxaki zenkqubo ekuvelisweni kweengxowa zefoyile ye-aluminiyam
Ubushushu bokungena kwetonela yokomisa buphezulu kakhulu okanye akukho gradient yobushushu, ubushushu bokungena buphezulu kakhulu, kwaye ukomisa kukhawuleze kakhulu, kangangokuba isinyibilikisi esikumphezulu weleyara yeglu siyaphela ngokukhawuleza, umphezulu uyaqhekeka, kwaye emva koko xa ubushushu bungena kwileyara yeglu, igesi yesinyibilikisi engaphantsi kwefilimu Iyaphula ifilimu yerabha ukuze yenze isangqa esifana ne-volcanic crater, kwaye izangqa zenza umaleko werabha ungacaci.
Kukho uthuli oluninzi kakhulu kumgangatho wokusingqongileyo, kwaye kukho uthuli emva kokuncamathisela kwi-oven yombane emoyeni ofudumeleyo, olunamathela kumphezulu we-viscose, kwaye ixesha elidibeneyo libekwe phakathi kweepleyiti zentsimbi ezisisiseko ezi-2. Indlela: Ukungena kungasebenzisa izihluzi ezininzi ukususa uthuli emoyeni ofudumeleyo.
Ubungakanani beglu alwanelanga, kukho indawo engenanto, kwaye kukho amaqamza omoya amancinci, abangela amabala okanye ukungacaci. Jonga ubungakanani beglu ukuze ibe yanele kwaye ifane

4